Thermal oxidation aging of rubbers: Characterization by chemiluminescence

Research output: Contribution to journalArticleResearchpeer review

Authors

  • M. Santoso
  • U. Giese
  • R. H. Schuster

External Research Organisations

  • German Institute of Rubber Technology (DIK e.V.)
View graph of relations

Details

Original languageEnglish
Pages (from-to)192-198
Number of pages7
JournalKGK Kautschuk Gummi Kunststoffe
Volume60
Issue number4
Publication statusPublished - Apr 2007
Externally publishedYes

Abstract

The investigations of thermal-oxidative aging on polydienes with systematic varied microstructure showed that high concentrations of double bonds in the polymer backbone play the significant role. From the shift of OIT-values it is observed, that styrene units have a relatively more stabilizing effect than vinyl units. Semi-quantitative infrared spectroscopic measurements taken during the course of CL analysis show much higher reactivity for 1,4-butadiene-units in comparison to vinyl. The kinetic evaluation of the CL curves results in rising reaction rate constants with increasing temperature and leads to activation energy values consistent with the reactivity of the polymers. In the investigations on the influence of processing it could be observed, that the raw polymer stabilizer is consumed during milling due to the effect of temperature, shearing and oxygen.

Keywords

    Chemiluminescence, Polydienes, Thermal oxidative aging

ASJC Scopus subject areas

Cite this

Thermal oxidation aging of rubbers: Characterization by chemiluminescence. / Santoso, M.; Giese, U.; Schuster, R. H.
In: KGK Kautschuk Gummi Kunststoffe, Vol. 60, No. 4, 04.2007, p. 192-198.

Research output: Contribution to journalArticleResearchpeer review

Santoso, M, Giese, U & Schuster, RH 2007, 'Thermal oxidation aging of rubbers: Characterization by chemiluminescence', KGK Kautschuk Gummi Kunststoffe, vol. 60, no. 4, pp. 192-198.
Santoso, M. ; Giese, U. ; Schuster, R. H. / Thermal oxidation aging of rubbers : Characterization by chemiluminescence. In: KGK Kautschuk Gummi Kunststoffe. 2007 ; Vol. 60, No. 4. pp. 192-198.
Download
@article{0f47c8fdc9194230a84fe54a2b7d1128,
title = "Thermal oxidation aging of rubbers: Characterization by chemiluminescence",
abstract = "The investigations of thermal-oxidative aging on polydienes with systematic varied microstructure showed that high concentrations of double bonds in the polymer backbone play the significant role. From the shift of OIT-values it is observed, that styrene units have a relatively more stabilizing effect than vinyl units. Semi-quantitative infrared spectroscopic measurements taken during the course of CL analysis show much higher reactivity for 1,4-butadiene-units in comparison to vinyl. The kinetic evaluation of the CL curves results in rising reaction rate constants with increasing temperature and leads to activation energy values consistent with the reactivity of the polymers. In the investigations on the influence of processing it could be observed, that the raw polymer stabilizer is consumed during milling due to the effect of temperature, shearing and oxygen.",
keywords = "Chemiluminescence, Polydienes, Thermal oxidative aging",
author = "M. Santoso and U. Giese and Schuster, {R. H.}",
year = "2007",
month = apr,
language = "English",
volume = "60",
pages = "192--198",
journal = "KGK Kautschuk Gummi Kunststoffe",
issn = "0948-3276",
publisher = "Huethig GmbH & Co. KG",
number = "4",

}

Download

TY - JOUR

T1 - Thermal oxidation aging of rubbers

T2 - Characterization by chemiluminescence

AU - Santoso, M.

AU - Giese, U.

AU - Schuster, R. H.

PY - 2007/4

Y1 - 2007/4

N2 - The investigations of thermal-oxidative aging on polydienes with systematic varied microstructure showed that high concentrations of double bonds in the polymer backbone play the significant role. From the shift of OIT-values it is observed, that styrene units have a relatively more stabilizing effect than vinyl units. Semi-quantitative infrared spectroscopic measurements taken during the course of CL analysis show much higher reactivity for 1,4-butadiene-units in comparison to vinyl. The kinetic evaluation of the CL curves results in rising reaction rate constants with increasing temperature and leads to activation energy values consistent with the reactivity of the polymers. In the investigations on the influence of processing it could be observed, that the raw polymer stabilizer is consumed during milling due to the effect of temperature, shearing and oxygen.

AB - The investigations of thermal-oxidative aging on polydienes with systematic varied microstructure showed that high concentrations of double bonds in the polymer backbone play the significant role. From the shift of OIT-values it is observed, that styrene units have a relatively more stabilizing effect than vinyl units. Semi-quantitative infrared spectroscopic measurements taken during the course of CL analysis show much higher reactivity for 1,4-butadiene-units in comparison to vinyl. The kinetic evaluation of the CL curves results in rising reaction rate constants with increasing temperature and leads to activation energy values consistent with the reactivity of the polymers. In the investigations on the influence of processing it could be observed, that the raw polymer stabilizer is consumed during milling due to the effect of temperature, shearing and oxygen.

KW - Chemiluminescence

KW - Polydienes

KW - Thermal oxidative aging

UR - http://www.scopus.com/inward/record.url?scp=34247558255&partnerID=8YFLogxK

M3 - Article

AN - SCOPUS:34247558255

VL - 60

SP - 192

EP - 198

JO - KGK Kautschuk Gummi Kunststoffe

JF - KGK Kautschuk Gummi Kunststoffe

SN - 0948-3276

IS - 4

ER -