Weakening of thick steel plates by laser radiation for the removal of hazardous substances

Publikation: Beitrag in FachzeitschriftKonferenzaufsatz in FachzeitschriftForschungPeer-Review

Autoren

  • Christian Hoff
  • Jörg Hermsdorf
  • Stefan Kaierle
  • Ludger Overmeyer

Externe Organisationen

  • Laser Zentrum Hannover e.V. (LZH)
Forschungs-netzwerk anzeigen

Details

OriginalspracheEnglisch
Seiten (von - bis)425-429
Seitenumfang5
FachzeitschriftProcedia CIRP
Jahrgang74
PublikationsstatusVeröffentlicht - 3 Sept. 2018
Extern publiziertJa
Veranstaltung10th CIRP Conference on Photonic Technologies, LANE 2018 - Furth, Deutschland
Dauer: 3 Sept. 20186 Sept. 2018

Abstract

Hazardous substances such as unexploded ordnance represent a serious threat. It is necessary to develop new methods and equipment for their elimination. For this reason, a laser ablation process is developed where the shell of the objects are weakened in a defined manner to reduce the threat to the environment. This article shows how 25 mm thick steel sheets can be weakened with ablation rates of more than 3000 mm3/min and achieved ablation depths of more than 15 mm by means of an adapted process strategy and an off-axis process gas control. Despite the high incoming process energy, it is ensured that there is no danger to affect the hazardous substances. A critical temperature of 300 °C is not exceeded at the rear surface of the sheet metal.

ASJC Scopus Sachgebiete

Zitieren

Weakening of thick steel plates by laser radiation for the removal of hazardous substances. / Hoff, Christian; Hermsdorf, Jörg; Kaierle, Stefan et al.
in: Procedia CIRP, Jahrgang 74, 03.09.2018, S. 425-429.

Publikation: Beitrag in FachzeitschriftKonferenzaufsatz in FachzeitschriftForschungPeer-Review

Hoff, C, Hermsdorf, J, Kaierle, S & Overmeyer, L 2018, 'Weakening of thick steel plates by laser radiation for the removal of hazardous substances', Procedia CIRP, Jg. 74, S. 425-429. https://doi.org/10.1016/j.procir.2018.08.166
Hoff, C., Hermsdorf, J., Kaierle, S., & Overmeyer, L. (2018). Weakening of thick steel plates by laser radiation for the removal of hazardous substances. Procedia CIRP, 74, 425-429. https://doi.org/10.1016/j.procir.2018.08.166
Hoff C, Hermsdorf J, Kaierle S, Overmeyer L. Weakening of thick steel plates by laser radiation for the removal of hazardous substances. Procedia CIRP. 2018 Sep 3;74:425-429. doi: 10.1016/j.procir.2018.08.166
Hoff, Christian ; Hermsdorf, Jörg ; Kaierle, Stefan et al. / Weakening of thick steel plates by laser radiation for the removal of hazardous substances. in: Procedia CIRP. 2018 ; Jahrgang 74. S. 425-429.
Download
@article{e32e86904a1d4e48a8375bb1f92b0e59,
title = "Weakening of thick steel plates by laser radiation for the removal of hazardous substances",
abstract = "Hazardous substances such as unexploded ordnance represent a serious threat. It is necessary to develop new methods and equipment for their elimination. For this reason, a laser ablation process is developed where the shell of the objects are weakened in a defined manner to reduce the threat to the environment. This article shows how 25 mm thick steel sheets can be weakened with ablation rates of more than 3000 mm3/min and achieved ablation depths of more than 15 mm by means of an adapted process strategy and an off-axis process gas control. Despite the high incoming process energy, it is ensured that there is no danger to affect the hazardous substances. A critical temperature of 300 °C is not exceeded at the rear surface of the sheet metal.",
keywords = "High speed ablation, Laser ablation, Macro metal weakening, Thick metal processing",
author = "Christian Hoff and J{\"o}rg Hermsdorf and Stefan Kaierle and Ludger Overmeyer",
note = "Funding information: The project underlying this report was funded by the German Federal Ministry of Education and Research under founding reference 13N14155. The authors thank for the support.; 10th CIRP Conference on Photonic Technologies, LANE 2018 ; Conference date: 03-09-2018 Through 06-09-2018",
year = "2018",
month = sep,
day = "3",
doi = "10.1016/j.procir.2018.08.166",
language = "English",
volume = "74",
pages = "425--429",

}

Download

TY - JOUR

T1 - Weakening of thick steel plates by laser radiation for the removal of hazardous substances

AU - Hoff, Christian

AU - Hermsdorf, Jörg

AU - Kaierle, Stefan

AU - Overmeyer, Ludger

N1 - Funding information: The project underlying this report was funded by the German Federal Ministry of Education and Research under founding reference 13N14155. The authors thank for the support.

PY - 2018/9/3

Y1 - 2018/9/3

N2 - Hazardous substances such as unexploded ordnance represent a serious threat. It is necessary to develop new methods and equipment for their elimination. For this reason, a laser ablation process is developed where the shell of the objects are weakened in a defined manner to reduce the threat to the environment. This article shows how 25 mm thick steel sheets can be weakened with ablation rates of more than 3000 mm3/min and achieved ablation depths of more than 15 mm by means of an adapted process strategy and an off-axis process gas control. Despite the high incoming process energy, it is ensured that there is no danger to affect the hazardous substances. A critical temperature of 300 °C is not exceeded at the rear surface of the sheet metal.

AB - Hazardous substances such as unexploded ordnance represent a serious threat. It is necessary to develop new methods and equipment for their elimination. For this reason, a laser ablation process is developed where the shell of the objects are weakened in a defined manner to reduce the threat to the environment. This article shows how 25 mm thick steel sheets can be weakened with ablation rates of more than 3000 mm3/min and achieved ablation depths of more than 15 mm by means of an adapted process strategy and an off-axis process gas control. Despite the high incoming process energy, it is ensured that there is no danger to affect the hazardous substances. A critical temperature of 300 °C is not exceeded at the rear surface of the sheet metal.

KW - High speed ablation

KW - Laser ablation

KW - Macro metal weakening

KW - Thick metal processing

UR - http://www.scopus.com/inward/record.url?scp=85057408987&partnerID=8YFLogxK

U2 - 10.1016/j.procir.2018.08.166

DO - 10.1016/j.procir.2018.08.166

M3 - Conference article

AN - SCOPUS:85057408987

VL - 74

SP - 425

EP - 429

JO - Procedia CIRP

JF - Procedia CIRP

SN - 2212-8271

T2 - 10th CIRP Conference on Photonic Technologies, LANE 2018

Y2 - 3 September 2018 through 6 September 2018

ER -