Abstract

Multi-material-designed components allow engineers to compose each zone of a component with the most qualified material in accordance with local demands.

In machining of multi-material-designed components new challenges arise. Significant shape deviations of workpiece surfaces occur that do not occur in machining of single materials. Surface shape deviations are an important quality aspect concerning further assembly of parts or functionality in service.

The identification of causes requires the holistic consideration of the interaction between machine tool, cutting tool, workpiece material properties, process parameters and process strategy. Characteristic shape deviations are identified in dependence of their cause. The machined surface shape is predicted using mechanical, semi-empirical and numerical models. Surface imperfections are analyzed experimentally. Finally, guidelines for the improvement of the surface quality are compiled to prevent wastage and refining operations.

Zitieren

Surface shape deviations in face milling of multi-material-designed components. / Hasselberg, Eike.
2021. 173 S.

Publikation: Qualifikations-/StudienabschlussarbeitDissertation

Hasselberg E. Surface shape deviations in face milling of multi-material-designed components. 2021. 173 S. (Berichte aus dem IFW).
Download
@phdthesis{a3df45ef60264adeb2bfd75c7bd83af5,
title = "Surface shape deviations in face milling of multi-material-designed components",
abstract = "Multi-material-designed components allow engineers to compose each zone of a component with the most qualified material in accordance with local demands.In machining of multi-material-designed components new challenges arise. Significant shape deviations of workpiece surfaces occur that do not occur in machining of single materials. Surface shape deviations are an important quality aspect concerning further assembly of parts or functionality in service.The identification of causes requires the holistic consideration of the interaction between machine tool, cutting tool, workpiece material properties, process parameters and process strategy. Characteristic shape deviations are identified in dependence of their cause. The machined surface shape is predicted using mechanical, semi-empirical and numerical models. Surface imperfections are analyzed experimentally. Finally, guidelines for the improvement of the surface quality are compiled to prevent wastage and refining operations.",
keywords = "multi-material machining, face milling, material compound, shape deviations, surface quality",
author = "Eike Hasselberg",
note = "Doctoral thesis",
year = "2021",
language = "English",
isbn = "978-3-95900-549-4",
volume = "02/2021",
series = "Berichte aus dem IFW",

}

Download

TY - BOOK

T1 - Surface shape deviations in face milling of multi-material-designed components

AU - Hasselberg, Eike

N1 - Doctoral thesis

PY - 2021

Y1 - 2021

N2 - Multi-material-designed components allow engineers to compose each zone of a component with the most qualified material in accordance with local demands.In machining of multi-material-designed components new challenges arise. Significant shape deviations of workpiece surfaces occur that do not occur in machining of single materials. Surface shape deviations are an important quality aspect concerning further assembly of parts or functionality in service.The identification of causes requires the holistic consideration of the interaction between machine tool, cutting tool, workpiece material properties, process parameters and process strategy. Characteristic shape deviations are identified in dependence of their cause. The machined surface shape is predicted using mechanical, semi-empirical and numerical models. Surface imperfections are analyzed experimentally. Finally, guidelines for the improvement of the surface quality are compiled to prevent wastage and refining operations.

AB - Multi-material-designed components allow engineers to compose each zone of a component with the most qualified material in accordance with local demands.In machining of multi-material-designed components new challenges arise. Significant shape deviations of workpiece surfaces occur that do not occur in machining of single materials. Surface shape deviations are an important quality aspect concerning further assembly of parts or functionality in service.The identification of causes requires the holistic consideration of the interaction between machine tool, cutting tool, workpiece material properties, process parameters and process strategy. Characteristic shape deviations are identified in dependence of their cause. The machined surface shape is predicted using mechanical, semi-empirical and numerical models. Surface imperfections are analyzed experimentally. Finally, guidelines for the improvement of the surface quality are compiled to prevent wastage and refining operations.

KW - multi-material machining, face milling, material compound, shape deviations, surface quality

M3 - Doctoral thesis

SN - 978-3-95900-549-4

VL - 02/2021

T3 - Berichte aus dem IFW

ER -