Research of the structure defects at wire-feed laser and laser-arc deposition with almg6

Publikation: Beitrag in FachzeitschriftKonferenzaufsatz in FachzeitschriftForschungPeer-Review

Autorschaft

  • A. A. Voropaev
  • A. D. Akhmetov
  • T. Hassel
  • G. G. Klimov

Organisationseinheiten

Externe Organisationen

  • St. Petersburg State Polytechnical University
  • Sankt-Peterburgskiy Gosudarstvennyy Morskoy Tekhnicheskiy Universitet (SMTU)
Forschungs-netzwerk anzeigen

Details

OriginalspracheEnglisch
Seiten (von - bis)504-511
Seitenumfang8
FachzeitschriftKey Engineering Materials
Jahrgang822
Frühes Online-Datum24 Sept. 2019
PublikationsstatusVeröffentlicht - 2019
VeranstaltungInternational Scientific Conference on New Materials and Technologies in Mechanical Engineering, NMTME 2019 - St. Petersburg, Russland
Dauer: 12 März 201915 März 2019

Abstract

In comparison with other additive methods, the wire additive manufacturing has some advantages, chief among: high deposition rate and low price for consumables. Otherwise there are some disadvantages such as a high level of internal defects (hot, cold cracks, pores). Adding laser radiation to a WAAM process can significantly reduce data flaws. In this paper outlined research results on the effect of laser radiation (pulsed and permanent) on structure and internal defects of deposit layers to create three-component structures from AlMg6 alloy. Reported samples was made by using hybrid laser-arc method and by applying a single laser. Presented photos of macrosections of obtained samples. Spectral analysis was performed to identify the nature of changes of grains in different processes. Were made the measurements of internal defects and chemical analysis of the obtained walls.

ASJC Scopus Sachgebiete

Zitieren

Research of the structure defects at wire-feed laser and laser-arc deposition with almg6. / Voropaev, A. A.; Akhmetov, A. D.; Hassel, T. et al.
in: Key Engineering Materials, Jahrgang 822, 2019, S. 504-511.

Publikation: Beitrag in FachzeitschriftKonferenzaufsatz in FachzeitschriftForschungPeer-Review

Voropaev, AA, Akhmetov, AD, Hassel, T & Klimov, GG 2019, 'Research of the structure defects at wire-feed laser and laser-arc deposition with almg6', Key Engineering Materials, Jg. 822, S. 504-511. https://doi.org/10.4028/www.scientific.net/KEM.822.504
Voropaev, A. A., Akhmetov, A. D., Hassel, T., & Klimov, G. G. (2019). Research of the structure defects at wire-feed laser and laser-arc deposition with almg6. Key Engineering Materials, 822, 504-511. https://doi.org/10.4028/www.scientific.net/KEM.822.504
Voropaev AA, Akhmetov AD, Hassel T, Klimov GG. Research of the structure defects at wire-feed laser and laser-arc deposition with almg6. Key Engineering Materials. 2019;822:504-511. Epub 2019 Sep 24. doi: 10.4028/www.scientific.net/KEM.822.504
Voropaev, A. A. ; Akhmetov, A. D. ; Hassel, T. et al. / Research of the structure defects at wire-feed laser and laser-arc deposition with almg6. in: Key Engineering Materials. 2019 ; Jahrgang 822. S. 504-511.
Download
@article{56ba7174dee84f5a899da4ec86cc4552,
title = "Research of the structure defects at wire-feed laser and laser-arc deposition with almg6",
abstract = "In comparison with other additive methods, the wire additive manufacturing has some advantages, chief among: high deposition rate and low price for consumables. Otherwise there are some disadvantages such as a high level of internal defects (hot, cold cracks, pores). Adding laser radiation to a WAAM process can significantly reduce data flaws. In this paper outlined research results on the effect of laser radiation (pulsed and permanent) on structure and internal defects of deposit layers to create three-component structures from AlMg6 alloy. Reported samples was made by using hybrid laser-arc method and by applying a single laser. Presented photos of macrosections of obtained samples. Spectral analysis was performed to identify the nature of changes of grains in different processes. Were made the measurements of internal defects and chemical analysis of the obtained walls.",
keywords = "Hybrid laser arc technology, MIG torch, Pulse laser mode, Wire and laser additive manufacturing, СW laser mode",
author = "Voropaev, {A. A.} and Akhmetov, {A. D.} and T. Hassel and Klimov, {G. G.}",
year = "2019",
doi = "10.4028/www.scientific.net/KEM.822.504",
language = "English",
volume = "822",
pages = "504--511",
note = "International Scientific Conference on New Materials and Technologies in Mechanical Engineering, NMTME 2019 ; Conference date: 12-03-2019 Through 15-03-2019",

}

Download

TY - JOUR

T1 - Research of the structure defects at wire-feed laser and laser-arc deposition with almg6

AU - Voropaev, A. A.

AU - Akhmetov, A. D.

AU - Hassel, T.

AU - Klimov, G. G.

PY - 2019

Y1 - 2019

N2 - In comparison with other additive methods, the wire additive manufacturing has some advantages, chief among: high deposition rate and low price for consumables. Otherwise there are some disadvantages such as a high level of internal defects (hot, cold cracks, pores). Adding laser radiation to a WAAM process can significantly reduce data flaws. In this paper outlined research results on the effect of laser radiation (pulsed and permanent) on structure and internal defects of deposit layers to create three-component structures from AlMg6 alloy. Reported samples was made by using hybrid laser-arc method and by applying a single laser. Presented photos of macrosections of obtained samples. Spectral analysis was performed to identify the nature of changes of grains in different processes. Were made the measurements of internal defects and chemical analysis of the obtained walls.

AB - In comparison with other additive methods, the wire additive manufacturing has some advantages, chief among: high deposition rate and low price for consumables. Otherwise there are some disadvantages such as a high level of internal defects (hot, cold cracks, pores). Adding laser radiation to a WAAM process can significantly reduce data flaws. In this paper outlined research results on the effect of laser radiation (pulsed and permanent) on structure and internal defects of deposit layers to create three-component structures from AlMg6 alloy. Reported samples was made by using hybrid laser-arc method and by applying a single laser. Presented photos of macrosections of obtained samples. Spectral analysis was performed to identify the nature of changes of grains in different processes. Were made the measurements of internal defects and chemical analysis of the obtained walls.

KW - Hybrid laser arc technology

KW - MIG torch

KW - Pulse laser mode

KW - Wire and laser additive manufacturing

KW - СW laser mode

UR - http://www.scopus.com/inward/record.url?scp=85106037159&partnerID=8YFLogxK

U2 - 10.4028/www.scientific.net/KEM.822.504

DO - 10.4028/www.scientific.net/KEM.822.504

M3 - Conference article

AN - SCOPUS:85106037159

VL - 822

SP - 504

EP - 511

JO - Key Engineering Materials

JF - Key Engineering Materials

SN - 1013-9826

T2 - International Scientific Conference on New Materials and Technologies in Mechanical Engineering, NMTME 2019

Y2 - 12 March 2019 through 15 March 2019

ER -