Determination of the flow behavior of the joining zones of hybrid semi-finished products by means of nanoindentation. Düsseldorf, Germany, Nanobruecken 2020, Nanomechanical Testing Conference & Bruker Hysitron User Meeting

Publikation: Buch/Bericht/Sammelwerk/KonferenzbandKonferenzbandForschung

Forschungs-netzwerk anzeigen

Details

OriginalspracheDeutsch
PublikationsstatusVeröffentlicht - 2020

Zitieren

Download
@book{6926ca2dab724994b650e39ab0af9e1e,
title = "Determination of the flow behavior of the joining zones of hybrid semi-finished products by means of nanoindentation.: D{\"u}sseldorf, Germany, Nanobruecken 2020, Nanomechanical Testing Conference & Bruker Hysitron User Meeting",
author = "Tim Matthias and Norman Heimes and Florian Pape and Bernd-Arno Behrens",
year = "2020",
language = "Deutsch",

}

Download

TY - BOOK

T1 - Determination of the flow behavior of the joining zones of hybrid semi-finished products by means of nanoindentation.

T2 - Düsseldorf, Germany, Nanobruecken 2020, Nanomechanical Testing Conference & Bruker Hysitron User Meeting

AU - Matthias, Tim

AU - Heimes, Norman

AU - Pape, Florian

AU - Behrens, Bernd-Arno

PY - 2020

Y1 - 2020

M3 - Konferenzband

BT - Determination of the flow behavior of the joining zones of hybrid semi-finished products by means of nanoindentation.

ER -

Von denselben Autoren