Abstract
For the improvement of properties ionic liquids (iL) in different concentrations were incorporated in fluorinated rubber (Fpm) and hydrogenated acrylonitrilebutadiene rubber (HNBr). different types of iLs were used based on imidazolium and pyrrolidinium cations. The scope of this work was to identify structure- property relationships. Compared to the raw polymer significant lower glass transition temperatures (Tg) and lower viscosity were observed for Fpm / iL - and HNBr / iL - systems in dependency of the iL- structure. Stress-strain measurements on elastomers with iL result in solely minor reduced values of tensile strength.
ASJC Scopus Sachgebiete
- Ingenieurwesen (insg.)
- Maschinenbau
- Werkstoffwissenschaften (insg.)
- Polymere und Kunststoffe
- Ingenieurwesen (insg.)
- Wirtschaftsingenieurwesen und Fertigungstechnik
- Werkstoffwissenschaften (insg.)
- Werkstoffchemie
Zitieren
- Standard
- Harvard
- Apa
- Vancouver
- BibTex
- RIS
in: KGK Kautschuk Gummi Kunststoffe, Jahrgang 69, Nr. 3, 03.2016, S. 38-45.
Publikation: Beitrag in Fachzeitschrift › Artikel › Forschung › Peer-Review
}
TY - JOUR
T1 - Customized performance modification of Special rubbers using ionic liquids
AU - Lückmann, M.
AU - Schuster, R. H.
AU - Giese, U.
PY - 2016/3
Y1 - 2016/3
N2 - For the improvement of properties ionic liquids (iL) in different concentrations were incorporated in fluorinated rubber (Fpm) and hydrogenated acrylonitrilebutadiene rubber (HNBr). different types of iLs were used based on imidazolium and pyrrolidinium cations. The scope of this work was to identify structure- property relationships. Compared to the raw polymer significant lower glass transition temperatures (Tg) and lower viscosity were observed for Fpm / iL - and HNBr / iL - systems in dependency of the iL- structure. Stress-strain measurements on elastomers with iL result in solely minor reduced values of tensile strength.
AB - For the improvement of properties ionic liquids (iL) in different concentrations were incorporated in fluorinated rubber (Fpm) and hydrogenated acrylonitrilebutadiene rubber (HNBr). different types of iLs were used based on imidazolium and pyrrolidinium cations. The scope of this work was to identify structure- property relationships. Compared to the raw polymer significant lower glass transition temperatures (Tg) and lower viscosity were observed for Fpm / iL - and HNBr / iL - systems in dependency of the iL- structure. Stress-strain measurements on elastomers with iL result in solely minor reduced values of tensile strength.
KW - Fluorinated rubber (FPM)
KW - Free volume
KW - Glass transition temperature (TG)
KW - Hydrogenated acrylonitrile-butadiene rubber (HNBR)
KW - Ionic liquid (IL)
UR - http://www.scopus.com/inward/record.url?scp=85019177620&partnerID=8YFLogxK
M3 - Article
AN - SCOPUS:85019177620
VL - 69
SP - 38
EP - 45
JO - KGK Kautschuk Gummi Kunststoffe
JF - KGK Kautschuk Gummi Kunststoffe
SN - 0948-3276
IS - 3
ER -