Comparison of different catalysts in the membrane-supported dehydrogenation of propane

Publikation: Beitrag in FachzeitschriftArtikelForschungPeer-Review

Autoren

  • R. Schäfer
  • M. Noack
  • P. Kölsch
  • M. Stöhr
  • J. Caro

Externe Organisationen

  • Leibniz-Institut für Katalyse e. V. an der Universität Rostock (LIKAT)
Forschungs-netzwerk anzeigen

Details

OriginalspracheEnglisch
Seiten (von - bis)15-23
Seitenumfang9
FachzeitschriftCatalysis today
Jahrgang82
Ausgabenummer1-4
Frühes Online-Datum25 Juni 2003
PublikationsstatusVeröffentlicht - 30 Juli 2003

Abstract

Dehydrogenation of propane is studied in a high temperature packed bed catalytic membrane reactor with a hydrogen-selective silica membrane. The silica membrane is prepared by a two-step sol-gel process. The removal of hydrogen in the membrane reactor results in higher propane conversion and higher propene yields in comparison to an equivalent fixed-bed reactor. Unfortunately, as a result of the H2 removal coking is favoured in the membrane reactor. Therefore, the higher propene yields are found only for the first 100-120min time on stream. However, the lower selectivity of the membrane reactor due to coking is compensated to some extend by a reduced hydrogenolysis. Two commercial dehydrogenation catalysts of different activity were tested in the membrane reactor: Cr2O3/Al2O3 and Pt-Sn/Al2O3. The two catalysts show a different activity, coking, and regeneration behaviour in the membrane-supported propane dehydrogenation.

ASJC Scopus Sachgebiete

Zitieren

Comparison of different catalysts in the membrane-supported dehydrogenation of propane. / Schäfer, R.; Noack, M.; Kölsch, P. et al.
in: Catalysis today, Jahrgang 82, Nr. 1-4, 30.07.2003, S. 15-23.

Publikation: Beitrag in FachzeitschriftArtikelForschungPeer-Review

Schäfer R, Noack M, Kölsch P, Stöhr M, Caro J. Comparison of different catalysts in the membrane-supported dehydrogenation of propane. Catalysis today. 2003 Jul 30;82(1-4):15-23. Epub 2003 Jun 25. doi: 10.1016/S0920-5861(03)00198-6
Schäfer, R. ; Noack, M. ; Kölsch, P. et al. / Comparison of different catalysts in the membrane-supported dehydrogenation of propane. in: Catalysis today. 2003 ; Jahrgang 82, Nr. 1-4. S. 15-23.
Download
@article{129e69ea1539424b9cc861e74e36962b,
title = "Comparison of different catalysts in the membrane-supported dehydrogenation of propane",
abstract = "Dehydrogenation of propane is studied in a high temperature packed bed catalytic membrane reactor with a hydrogen-selective silica membrane. The silica membrane is prepared by a two-step sol-gel process. The removal of hydrogen in the membrane reactor results in higher propane conversion and higher propene yields in comparison to an equivalent fixed-bed reactor. Unfortunately, as a result of the H2 removal coking is favoured in the membrane reactor. Therefore, the higher propene yields are found only for the first 100-120min time on stream. However, the lower selectivity of the membrane reactor due to coking is compensated to some extend by a reduced hydrogenolysis. Two commercial dehydrogenation catalysts of different activity were tested in the membrane reactor: Cr2O3/Al2O3 and Pt-Sn/Al2O3. The two catalysts show a different activity, coking, and regeneration behaviour in the membrane-supported propane dehydrogenation.",
keywords = "Membrane reactor, Propane dehydrogenation, Silica membrane",
author = "R. Sch{\"a}fer and M. Noack and P. K{\"o}lsch and M. St{\"o}hr and J. Caro",
year = "2003",
month = jul,
day = "30",
doi = "10.1016/S0920-5861(03)00198-6",
language = "English",
volume = "82",
pages = "15--23",
journal = "Catalysis today",
issn = "0920-5861",
publisher = "Elsevier",
number = "1-4",

}

Download

TY - JOUR

T1 - Comparison of different catalysts in the membrane-supported dehydrogenation of propane

AU - Schäfer, R.

AU - Noack, M.

AU - Kölsch, P.

AU - Stöhr, M.

AU - Caro, J.

PY - 2003/7/30

Y1 - 2003/7/30

N2 - Dehydrogenation of propane is studied in a high temperature packed bed catalytic membrane reactor with a hydrogen-selective silica membrane. The silica membrane is prepared by a two-step sol-gel process. The removal of hydrogen in the membrane reactor results in higher propane conversion and higher propene yields in comparison to an equivalent fixed-bed reactor. Unfortunately, as a result of the H2 removal coking is favoured in the membrane reactor. Therefore, the higher propene yields are found only for the first 100-120min time on stream. However, the lower selectivity of the membrane reactor due to coking is compensated to some extend by a reduced hydrogenolysis. Two commercial dehydrogenation catalysts of different activity were tested in the membrane reactor: Cr2O3/Al2O3 and Pt-Sn/Al2O3. The two catalysts show a different activity, coking, and regeneration behaviour in the membrane-supported propane dehydrogenation.

AB - Dehydrogenation of propane is studied in a high temperature packed bed catalytic membrane reactor with a hydrogen-selective silica membrane. The silica membrane is prepared by a two-step sol-gel process. The removal of hydrogen in the membrane reactor results in higher propane conversion and higher propene yields in comparison to an equivalent fixed-bed reactor. Unfortunately, as a result of the H2 removal coking is favoured in the membrane reactor. Therefore, the higher propene yields are found only for the first 100-120min time on stream. However, the lower selectivity of the membrane reactor due to coking is compensated to some extend by a reduced hydrogenolysis. Two commercial dehydrogenation catalysts of different activity were tested in the membrane reactor: Cr2O3/Al2O3 and Pt-Sn/Al2O3. The two catalysts show a different activity, coking, and regeneration behaviour in the membrane-supported propane dehydrogenation.

KW - Membrane reactor

KW - Propane dehydrogenation

KW - Silica membrane

UR - http://www.scopus.com/inward/record.url?scp=17444438409&partnerID=8YFLogxK

U2 - 10.1016/S0920-5861(03)00198-6

DO - 10.1016/S0920-5861(03)00198-6

M3 - Article

AN - SCOPUS:17444438409

VL - 82

SP - 15

EP - 23

JO - Catalysis today

JF - Catalysis today

SN - 0920-5861

IS - 1-4

ER -