Aging processes of crosslinked polydienes and measures - Mechanisms and quantitative characterization

Publikation: Beitrag in FachzeitschriftArtikelForschungPeer-Review

Autoren

  • Inga Homeier
  • Yolanda Torrejon
  • Ulrich Giese

Externe Organisationen

  • Deutsches Institut für Kautschuktechnologie e.V. (DIK)
Forschungs-netzwerk anzeigen

Details

OriginalspracheEnglisch
Seiten (von - bis)44-51
Seitenumfang8
FachzeitschriftKGK Kautschuk Gummi Kunststoffe
Jahrgang70
Ausgabenummer1-2
PublikationsstatusVeröffentlicht - 1 Jan. 2017
Extern publiziertJa

Abstract

Thermal oxidative aging is limiting the life time of rubber products. Beside environmental factors the microstructure of used polymers, the crosslinking, fillers and additives are influencing components, especially several antioxidants, where their efficiency is of high interest. From the measurements using NMR-relaxation, CL and physical testing, it is to conclude, that the concentration of the C=C-double bonds in the main chain of the polymer has a significant quantitative influence on the thermal oxidative stability. The crosslink density has nearly no effect in the used SBR-systems. The investigations of the efficiency of antioxidants in IR and SBR with different micro structures results in the sequence DPPD > 6PPD > 77PD.

ASJC Scopus Sachgebiete

Zitieren

Aging processes of crosslinked polydienes and measures - Mechanisms and quantitative characterization. / Homeier, Inga; Torrejon, Yolanda; Giese, Ulrich.
in: KGK Kautschuk Gummi Kunststoffe, Jahrgang 70, Nr. 1-2, 01.01.2017, S. 44-51.

Publikation: Beitrag in FachzeitschriftArtikelForschungPeer-Review

Homeier, Inga ; Torrejon, Yolanda ; Giese, Ulrich. / Aging processes of crosslinked polydienes and measures - Mechanisms and quantitative characterization. in: KGK Kautschuk Gummi Kunststoffe. 2017 ; Jahrgang 70, Nr. 1-2. S. 44-51.
Download
@article{c891e94e7c7e48779bda33f10a252bb6,
title = "Aging processes of crosslinked polydienes and measures - Mechanisms and quantitative characterization",
abstract = "Thermal oxidative aging is limiting the life time of rubber products. Beside environmental factors the microstructure of used polymers, the crosslinking, fillers and additives are influencing components, especially several antioxidants, where their efficiency is of high interest. From the measurements using NMR-relaxation, CL and physical testing, it is to conclude, that the concentration of the C=C-double bonds in the main chain of the polymer has a significant quantitative influence on the thermal oxidative stability. The crosslink density has nearly no effect in the used SBR-systems. The investigations of the efficiency of antioxidants in IR and SBR with different micro structures results in the sequence DPPD > 6PPD > 77PD.",
keywords = "Crosslinking, Polymer microstructure, SBR-vulcanizates, Thermal oxidative aging",
author = "Inga Homeier and Yolanda Torrejon and Ulrich Giese",
year = "2017",
month = jan,
day = "1",
language = "English",
volume = "70",
pages = "44--51",
journal = "KGK Kautschuk Gummi Kunststoffe",
issn = "0948-3276",
publisher = "Huethig GmbH & Co. KG",
number = "1-2",

}

Download

TY - JOUR

T1 - Aging processes of crosslinked polydienes and measures - Mechanisms and quantitative characterization

AU - Homeier, Inga

AU - Torrejon, Yolanda

AU - Giese, Ulrich

PY - 2017/1/1

Y1 - 2017/1/1

N2 - Thermal oxidative aging is limiting the life time of rubber products. Beside environmental factors the microstructure of used polymers, the crosslinking, fillers and additives are influencing components, especially several antioxidants, where their efficiency is of high interest. From the measurements using NMR-relaxation, CL and physical testing, it is to conclude, that the concentration of the C=C-double bonds in the main chain of the polymer has a significant quantitative influence on the thermal oxidative stability. The crosslink density has nearly no effect in the used SBR-systems. The investigations of the efficiency of antioxidants in IR and SBR with different micro structures results in the sequence DPPD > 6PPD > 77PD.

AB - Thermal oxidative aging is limiting the life time of rubber products. Beside environmental factors the microstructure of used polymers, the crosslinking, fillers and additives are influencing components, especially several antioxidants, where their efficiency is of high interest. From the measurements using NMR-relaxation, CL and physical testing, it is to conclude, that the concentration of the C=C-double bonds in the main chain of the polymer has a significant quantitative influence on the thermal oxidative stability. The crosslink density has nearly no effect in the used SBR-systems. The investigations of the efficiency of antioxidants in IR and SBR with different micro structures results in the sequence DPPD > 6PPD > 77PD.

KW - Crosslinking

KW - Polymer microstructure

KW - SBR-vulcanizates

KW - Thermal oxidative aging

UR - http://www.scopus.com/inward/record.url?scp=85019205872&partnerID=8YFLogxK

M3 - Article

AN - SCOPUS:85019205872

VL - 70

SP - 44

EP - 51

JO - KGK Kautschuk Gummi Kunststoffe

JF - KGK Kautschuk Gummi Kunststoffe

SN - 0948-3276

IS - 1-2

ER -