Abstract
In liquid Li-Bi, Li-Pb, Li-Sn and Li-Si alloys the spinlattice relaxation rate T1-1 of Β-active8Li (T1/2=0.8s) probe nuclei has been measured over wide concentration (c) and temperature (T) ranges. T1-1 is governed by hyperfine contact interaction with the conduction electrons. Near the compositions Li3Bi, Li4Pb, Li4Sn and Li4Si both (T1T)-1 and d(T1T)-1/dT versus c show marked extrema. These data, when combined with Knightshift and/or conductivity values, inform on the prolongation of the electron "residence time" and the reduction of the density of states at the Fermi surface. There is progressive tendency to electron localization and compound formation in the sequence Li4Pb, Li4Sn, Li3Bi with mainly ionic bonding in the case of liquid Li3Bi.
ASJC Scopus Sachgebiete
- Physik und Astronomie (insg.)
- Atom- und Molekularphysik sowie Optik
- Physik und Astronomie (insg.)
- Kern- und Hochenergiephysik
- Physik und Astronomie (insg.)
- Physik der kondensierten Materie
- Chemie (insg.)
- Physikalische und Theoretische Chemie
Zitieren
- Standard
- Harvard
- Apa
- Vancouver
- BibTex
- RIS
in: Hyperfine Interactions, Jahrgang 16, Nr. 1-4, 12.1983, S. 569-572.
Publikation: Beitrag in Fachzeitschrift › Artikel › Forschung › Peer-Review
}
TY - JOUR
T1 - 8Li spin relaxation in liquid Li alloys with compound-forming tendency
AU - Heitjans, P.
AU - Kiese, G.
AU - van Der Marel, C.
AU - Ackermann, H.
AU - Bader, B.
AU - Freiländer, P.
AU - Stöckmann, H. J.
PY - 1983/12
Y1 - 1983/12
N2 - In liquid Li-Bi, Li-Pb, Li-Sn and Li-Si alloys the spinlattice relaxation rate T1-1 of Β-active8Li (T1/2=0.8s) probe nuclei has been measured over wide concentration (c) and temperature (T) ranges. T1-1 is governed by hyperfine contact interaction with the conduction electrons. Near the compositions Li3Bi, Li4Pb, Li4Sn and Li4Si both (T1T)-1 and d(T1T)-1/dT versus c show marked extrema. These data, when combined with Knightshift and/or conductivity values, inform on the prolongation of the electron "residence time" and the reduction of the density of states at the Fermi surface. There is progressive tendency to electron localization and compound formation in the sequence Li4Pb, Li4Sn, Li3Bi with mainly ionic bonding in the case of liquid Li3Bi.
AB - In liquid Li-Bi, Li-Pb, Li-Sn and Li-Si alloys the spinlattice relaxation rate T1-1 of Β-active8Li (T1/2=0.8s) probe nuclei has been measured over wide concentration (c) and temperature (T) ranges. T1-1 is governed by hyperfine contact interaction with the conduction electrons. Near the compositions Li3Bi, Li4Pb, Li4Sn and Li4Si both (T1T)-1 and d(T1T)-1/dT versus c show marked extrema. These data, when combined with Knightshift and/or conductivity values, inform on the prolongation of the electron "residence time" and the reduction of the density of states at the Fermi surface. There is progressive tendency to electron localization and compound formation in the sequence Li4Pb, Li4Sn, Li3Bi with mainly ionic bonding in the case of liquid Li3Bi.
UR - http://www.scopus.com/inward/record.url?scp=34250153965&partnerID=8YFLogxK
U2 - 10.1007/BF02147317
DO - 10.1007/BF02147317
M3 - Article
AN - SCOPUS:34250153965
VL - 16
SP - 569
EP - 572
JO - Hyperfine Interactions
JF - Hyperfine Interactions
SN - 0304-3834
IS - 1-4
ER -